Problem Description: Wrong color of gold. Accepted standards: Not accepted |
|
Problem Description: Failure to evenly cover Accepted standards: Not accepted |
|
Problem Description: The outer layer had dents before gold plating due to human manipulation. Accepted standards: 1. No dents larger than 0.125 mm are allowed in important areas; 2. No dents larger than 0.25 mm are allowed in non-important areas. |
|
Problem Description: 1. The gold surface is contaminated; 2. Insufficient maintenance; 3. The storage time exceeds the time specified in the document. Accepted standards: Not accepted |
|
Problem Description: 1. The copper surface debris was not cleaned up during pre-treatment; 2. The nickel cylinder was not activated well. Accepted standards: Not accepted |
|
Problem Description: 1. Abnormal gold sinking parameters; 2. High concentration and high temperature of the chemical solution; 3. High nickel-gold content; 4. Staying in the tank for too long. Accepted standards: It is acceptable within the range of ±20% of the original spacing, or not exceeding 0.05mm (the smaller of the two). |
With our professional soldering technicians, #SMT process engineers and component procurement specialists, we can provide an affordable highly flexible assembly process with quick turnaround.#factory #pcbassembly #pcbmanufacturing #pcbprototy pic.twitter.com/tIgAldKFIG
— POE PCB/PCBA Manufacturer (@poe_pcba) August 27, 2024
Since 1996, POE has become a globally renowned PCB company, providing small to medium volume PCB/ PCBA manufacturing services.